Welding Procedure Qualification
Overview
Under CSA Standards W47.1, W47.2, W186 and W55.3, all CWB Certified companies are required to submit their welding procedures to the Íâ¹úÃÀŮɫÇ鯬 for review and approval in accordance with the governing standard. This must be done before the start of any work.
Welding Procedures Data Sheets (WPDSs)
As part of the certification process, companies are required to submit for the CWB's review and acceptance welding procedures data sheets (WPDSs) for welded joints used by the company in accordance with the requirements of a design standard.
The information contained in a WPDS shall include:
- the type of joint
- joint geometry
- welding position
- welding symbol
- welding consumables
- gas mixture, and
- the welding parameters that are to be used in making a weldment.
Related Links
Company certification to CSA W47.1, W47.2, W55.3 and W186. Welding Procedure Guide
A guide to the preparation of welding procedure data sheets Welding Engineer Courses
Discover courses for welding engineers from CWB education. Contact Us
Have questions? Contact us for assistance.
Procedures Review Process
All welding procedures shall be sent at procedures@cwbgroup.org.
You will get a reply confirming the reception of your email by CWB.
All welding procedures should be submitted in PDF and not secured.
A review letter will be sent when the review will be completed.
There are three possible outcomes:
- Welding procedures have been accepted
- Welding procedures requires qualification
- Welding procedures requires revision
Turnaround time is three working days.
When PQR results are completed, a review letter confirming the test results will be sent.
Corresponding welding procedures will then have to be revised as per the PQR and returned to the procedure department for final review/acceptance